JLY-04 Series Concrete high-efficiency pumping agent
Item | Index |
PH | 6-7 |
Slurry fluidity | ≥200mm |
chloridion | free |
Water reducing rate | 15%-30% |
■ The liquid dosage is 1.0%-2.5% of total cementitious materials.
■ Mixed with this product under the same water-cement ratio,can increase the slump of concrete by more than 10cm. Under the same amount of cement and the same slump, the strength of concrete can be increased by 40%-70% in three days, by 30%-60% in seven days, and by 25%-50% in 28 days.
■ The loss of slump over time is small, which can meet the long-distance transportation of commercial concrete.
■ Workability, water retention and cohesion are greatly improved, no delamination and no segregation.
■ Initially there is a retarding effect. It can reduce the early hydration and heat release rate of concrete, which is beneficial to the pouring of large-volume concrete.
■ The compressive strength, flexural resistance, tensile strength, impermeability and durability of concrete have been significantly improved.
Physical And Mechanical Properties of Concrete
Item | Factory technical indicators | Standard | |
slump increase(mm) | ≥120 | ≥100 | |
Atmospheric bleeding rate water ratio(%) | ≤50 | ≤90 | |
Pressure bleeding rate ratio(%) | ≤50 | ≤90 | |
Air content(%) | ≤4.0 | ≤4.5 | |
slump retention value(mm) | 30min | ≥160 | ≥150 |
60min | ≥130 | ≥120 | |
Compressive strength ratio (%) not less than | 3days | 95 | 90 |
7days | 100 | 90 | |
28days | 110 | 90 | |
Shrinkage ratio(%) | 28days | ≤125 | ≤135 |
Corrosion effect on steel bars | No rust |
■ Please follow the "Concrete Admixture Application Technical Specifications" for construction.
■ This product has retarding effect, and the dosage should be strictly controlled in field application
■ Experiments should be carried out when using this product for the first time or changing the type of cement to obtain the best technical effect and economic benefit.
■ This product is suitable for concrete construction under the environmental conditions of -1℃-50℃